Quote:
Originally Posted by Mur
Thanks, yeah i think i may have been dragging it abit.
Try to avoid it.. yet the electrode ends up touching the workpiece every so often.
Does this cause it to be more sunken?
|
na meant you should be dragging it,
its hard to explain in writing
just say you wanted to do a standard fillet weld
going from left to right along the plate
your electrode should be pointed a about 30 degrees to the left dragging it to the right
and there are electrodes that ya can just rest on the job instead of trying to feed it in all the time
ferracraft and ya can also do it with 16tc's
Hope that makes sense